Sterilization Q&A

2026-05-12

Sterilization Q&A

Medical Dialysis Paper

- Available in standard system paper and high-temperature self-adhesive types.
- Specifications: Common weights are 60g/m² and 70g/m².

Film Construction

- CPP/PE Layer: Ranging from 38µm to 40µm thickness.
- Total composite thickness: Approximately 50µm - 52µm.

PART 02: Common Issues

Abnormal phenomena during the sterilization process of self-sealing pouches:

Bursting

1. Overloading: Placing too many items in the steam sterilizer prevents proper pressure release during vacuum stages, leading to bursting.
2. Improper Placement: Pouches placed directly against the chamber wall can be damaged by high-temperature contact.
3. Contamination: Residual oil/lubricants on instruments can reach extremely high temperatures when heated, causing the film to melt and burst.

Seal and Indicator Performance

- Puncture Damage: Sharp instruments without protective tips can easily pierce the film.
- Indicator Abnormalities: Incomplete or unclear color changes in the chemical indicator strips.

PART 03: Recommendations for Use

Avoid overloading the sterilizer chamber to ensure balanced internal pressure.
Maintain adequate distance between pouches and the chamber walls or areas with condensate.
Ensure sealing equipment operates at consistent temperature and pressure settings.
Mandatory use of protective tips or guards for all sharp surgical instruments.
Store pouches in a strictly clean and dry environment.
Always inspect indicator color changes and seal integrity before use.
Maintain at least a 2.5cm safety margin between the instrument and the seal edges.